极限电流型氧传感器以其测量范围广、使用寿命长、无需参比气体、精度高和响应快等优点,已在汽车、工业锅炉等领域成为控制废气排放......
The Effect of Plasma Spraying Power on LSGM-Based Metal Supported Intermediate temperature Solid Oxi
The nickel-iron metal supported solid oxide fuel cells fabricated by atmospheric plasma spraying(APS)are heat treated in......
LSGM 样品在1300℃下烧结有第二相LaSrGa3O7 和LaSrGaO4,通过适量掺杂MOO3 明显降低样品第二相含量,相纯度、致密度和电导率都......
La_(0.9)Sr_(0.1)Ga_(0.8)Mg_(0.2)O_(3-δ)(LSGM) and La_(0.7)Sr_(0.3)Cr_(0.5)Mn_(0.5)O_(3-δ)(LSCM) powders were synthesiz......
采用丝网印刷技术制备了以La0.9Sr0.1Ga0.8Mg0.2O3-δ(LSGM,Sr、Mg双掺杂的LaGaO3)为固体电解质、NiO为敏感电极(SE)材料的电流型N......
采用丝网印刷技术制备了以La0.9Sr0.1Ga0.8Mg0.2O3-δ(LSGM,Sr、Mg双掺杂的LaGaO3)为固体电解质、NiO为敏感电极(SE)材料的电流型NO2传......
Study on Synthesis and Properties of Intermediate-Temperature Solid Electrolyte with Perovskite Stru
...
Solid oxide fuel cell is attracting more attention in recent years for its lower pollution emission and high energy conv......
用EDTA-硝酸盐法合成了中温固体氧化物燃料电池的电解质La0.8Sr0.2Ga0.85Mg0.15O3-δ(LSGM).BET法测定了前驱粉体的比表面积.XRD和DT......
采用射频磁控溅射法成功地在多孔La0.7Sr0.3Cr0.5Mn0.5O3-δ(LSCM7355)阳极基底上制备了致密的LSGM电解质薄膜层。研究结果表明,当溅......
固体氧化物燃料电池(SOFC)要求电解质在工作温度下必须要有足够高的氧离子导电性,并且在氧化和还原气氛下仍然保持着离子导电性。传统......
综述了有关Sr、Mg掺杂镓酸镧(LSGM)固体电解质的研究进展,分析了LSGM的合成、结构及导电性,描述了LSGM基础上掺杂其他金属离子的研究结......
用改进的柠檬酸法合成了具有钙钛矿结构的LSGM(La0.9Sr0.1Ga0.85Mg0.15O3-δ)和Co掺杂的LSGMC8.5(La0.9Sr0.1(Ga0.9Co0.1)0.85Mg0.15O3-δ).并从XR......
La0.9Sr0.1Ga0.8Mg0.2Ox(LSGM)粉体在1000-1500℃烧结4 h得到不同LSGM样品,对各样品进行了各项物理和电学特性测试。结果表明,样品的......
采用EDTA络合溶胶-凝胶法合成了中温固体氧化物燃料电池的电解质LSGM8282(La0.8Sr0.2Ga0.8-Mg0.2O3-δ)和LSGMF5(La0.8Sr0.2Ga0.8Mg0.15Fe......
采用了一种全新的化学方法(PVP溶液聚合法)成功制备出了La0.8Sr0.2Ga0.83Mg0.17O2.815粉末;研究了不同含量聚合载体(PVP)对结果的影响......
以硝酸盐为前驱体合成了具有钙钛矿结构的中温固体电解质La0.9Sr0.1Ga0.8Mg0.2O3-δ(LSGM)。用XRD和SEM分析了样品钙钛矿相的形成过......
回 回 产卜爹仇贱回——回 日E回。”。回祖 一回“。回干 肉果幻中 N_。NH lP7-ewwe--一”$ MN。W;- __._——————》 砧叫]们......
本文采用凝胶燃烧法制备La0.9Sr0.1Ga0.8Mg0.2O3-δ固体电解质(LSGM),讨论了溶液浓度、pH值、柠檬酸的加入量、加热温度等工艺条件......
在用固相反应法合成电解质材料Lao 9Sr0.1Gao.8Mgo.2Oa-δ(LSGM)的基础上,研制出中温固体氧化物燃料电池LSGM+NiO阳极基底;考察了......
采用柠檬酸盐法制备了La0.9Sr0.1Ga0.8Mg0.2O3-α(LSGM)粉体材料.TG和DTA分析表明,凝胶在265~309℃下分解为相应的氧化物.XRD测试表......